finishing.com -- The Home Page of the Finishing Industry
A website for Serious Education, promoting Aloha,
& the most FUN smiley you can have in metal finishing.
    no popups, no spam
HomeFAQsSuggested
Books
Help
Wanteds
Advertise
on this site
FORUM
current topics
topic 1487

Water-Glass coating to deter white rust on Zinc


(1998)

I have tried to create a system which enhances my corrosion resistance to white rust. So far, I am using various compositions of chromate + activators (with varying pH, time and Temperature conditions). After drying, I am applying a "water glass"-type of coating (produced by someone else).

...and now the question...Do you know what additives I can add to this water glass coating to aid in corrosion resistance? If you could direct me to a company that sells an additive or has information on this I would appreciate it very much.

Thank You in advance.--Jim

p.s. As best as I can tell the biggest problem thus far is the alkalinity and silicate content of the water glass to introduction of additives...HELP

Jim Wilkes
Madison Chemical



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Comment to THIS thread START a NEW threadView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.