Mercury damage to gold jewelry is discussed as an urgent problem that can quickly discolor, weaken, and even crack rings and other pieces. Several readers report that boiling the affected jewelry in coconut oil restored the gold color and removed the mercury contamination, including wedding and engagement rings. One commenter, Adam Efthimiou, says he is a chemist and jeweler and offers paid repair help, noting that small discoloration may be repairable but badly eaten-away pieces may need to be remade. Ted Mooney advises that the damage should be fixed immediately because it continues over time and can crack the ring; if cracking has already occurred, the crack will remain. A later question asks whether a ring damaged five days earlier can still be treated, and the answer is that coconut oil may still reduce further damage, but it cannot reverse existing cracks.




< Prev. page

        

(You’re on the last page of this topic)


Contact with mercury instantly ruins jewelry, but boiling it in coconut oil can fix it! Read on . . .

A. Hello all.

I see many of you are having issues with mercury ruining jewelry. I just so happen to be first a chemist and second a jeweler — still learning though! For anyone who has jewelry that hasn’t been completely destroyed and would like it repaired I’d be happy to do so. Worst case scenario if I can’t repair your item I will issue a full refund and mail back your jewelry, I am no expert jeweler by any means I’m more of a hobbyist but I am a chemist with my masters and full lab for handling these issues with ease. Small damage I can say comfortably I can repair but if half your ring is gone I hate to be the bearer of bad news, most likely it’s beyond repair short of melting down and making an entirely new piece.
Feel free to contact me and I’ll be glad to see what I can do to help. If it’s just a simple discoloration and no damage I can repair your jewelry for right around $30.00 US dollars; however, size has a lot to do with my time involved. I really hope I can help some of you for I too know how it feels to lose jewelry to mercury: my father gave me a beautiful 18kt gold ring with an onyx stone for graduating high school many years ago and I lost my ring from a broken mercury switch, aka thermostat. And my ring literally fell from my hand, malformed, which intrigued me to be a chemist and here I am today.

Adam efthimiou
Gold’N’Years 603-677-2254 – Ashland New Hampshire
February 11, 2015
^

Ed. note: As we said early on, it is a shame that professional jewelers tend to refuse to address this issue of mercury damage … because that refusal leads to inexperienced but desperate individuals attempting chemical treatments they are not trained or qualified to do! So, although this site is for technical discussions, not for commercial offerings or free ads … we’ve made an exception. But we don’t know Adam, and are neither recommending nor dis-recommending his service.

thumbs up signThanks to the website. Coconut oil really works.

malavika chakrabarty
– Kunming, China
February 22, 2015
^

thumbs up signApparently Coconut oil works 100%. Thanks.

nidhi shah
– mumbai india
April 5, 2015
^

thumbs up signTook out a broken thermometer from the medicine cabinet and the mercury was drawn like a magnet to my wedding and engagement ring which turned grey in font of my eyes, I was distraught. I looked on Google and found this site — so glad I did — decided to try as suggested put my rings in coconut oil after all I had nothing to lose, my rings were ruined. We put my rings in the oil in a foil container on the BBQ outside and it was amazing within 5 mins my rings were back to gold. Thank you so much.

Susan Druce
– West Byfleet, U.K.
June 22, 2015
^

A. I just tried a simple procedure today. I asked one of my friends, and he advised me. Heated up the gold using gas or others suitable for you and sinking into the water. Repeat it two or three times and clean the gold using brush & soap. I completely removed the mercury within 15 minutes. Take necessary precautions: Mercury is hazard to health, i.e., poison!
Good luck

Baiju km
– New Delhi, Delhi, India
August 8, 2015
^

thumbs up signToday my wife broke the thermo and started playing mercury like a kid :P , in a matter of seconds, the gold (wedding and one more) turned into silver color. Thanks a ton to the guys who posted this remedy; this remedy really works.

THANKS A LOT …Srini

Srinivas Pithani
– Bangalore, India
November 22, 2015
^

thumbs up signHello everyone,

I LOVE OUR SIMPLE COCONUT OIL.My new year was well started, but it turned out to be a disastrous one as my husband broke a thermometer yesterday and did not realise that some of the mercury fell into his drawer where he had kept his chain — (it is of 6 tholas approx., worth more than 1 n half lak). We were devastated today morning when we found his chain totally damaged and turned into silver color.I immediately searched google and find out this page. A million thanks to google and this page, this simple oil saved my loss of laks. I boiled the chain in coconut oil, maybe for 2 minutes, on my normal cooking gas stove in a steel vessel in my kitchen; chimney exhaust was on and my face except eyes were covered. Thick fumes came out, gradually chain turned into its original color. Steel vessel I simply disposed of.

Sobha panicker
– Delhi, india
January 3, 2016
^

thumbs up signThanks to Allah’s great gift coconut oil which restored my engagement ring diffused with mercury.

sabiha nasir
– pakistan
January 9, 2016
^

thumbs up signThank you so much…. The coconut oil thing worked out :)

Safa S.
– Amman, Jordan
March 7, 2016
^

thumbs up signThanks to this page .. Coconut oil trick worked out well to get rid of mercury on my wedding ring.

Ajith kodipelli
– Telangana, India
May 20, 2016
^

thumbs up signCoconut oil works … Thank you so much…

Subramanian iyer
– Navi mumbai, India
May 29, 2016
^


Q. There was a thread that spoke of mercury spreading through the ring- thus the ring appearing to return to dull gold colour. So the mercury is ‘diluted’? throughout the ring.
Does coconut boiling remove mercury only from surface blemishes or from ‘deeper within’ also?
So if the former dull/ silver ring is gold& shiny on the outside again after boiling, does that mean all the mercury that spread deeper in is out also?

Hanna Lubbe
– Swakopmund, Namibia
September 22, 2016
^


Q. How long can gold be left in the mercury after amalgamation? Can it be left indefinitely or should it processed as quickly as possible?

Ron Porter
– Flin Flon Mb Canada
June 1, 2017
^


Q. Don’t know what happened to my gold ring after I used beauty cream. One side turned to silver colour! After reading above experiences I understand that beauty cream contained mercury! I didn’t try coconut oil experiment … is it possible if stones are present in the ring?

Ihsana muneer
– Kerala,India
June 10, 2017
^


September 2017

A. Hi Ihsana. I’d be quite surprised if any beauty cream contained mercury. Boiling probably won’t hurt diamonds, but it’s probably not good for pearls and some other stones.

Regards,

ted_yosem
Ted Mooney, P.E. RET
Striving to live Aloha

finishing.com – Pine Beach, New Jersey



Need quick confidential answers? $25
Need project assistance? $100/hr.

^


Q. This happened to my ring 5 days ago and it cracked at one place is coconut oil still going to work? Please I need an answer quickly!

Tasneem Alkilany
– Cairo , Egypt
June 30, 2017
^


A. Hi Tasneem. It will minimize the continuing damage, so do it as soon as possible … but it can’t turn back time :-(

If the ring is cracked, it’s cracked. Best of luck with it though.

Regards,

ted_yosem
Ted Mooney, P.E. RET
Striving to live Aloha

finishing.com – Pine Beach, New Jersey



Need quick confidential answers? $25
Need project assistance? $100/hr.

June 2017
^


July 19, 2017

thumbs down signMy wife had a filling replaced at the dentist today and was wearing her bi-metallic Rolex
[affil link] watch.

When she got home, two or three of the gold middle links in the bracelet had gone a sort of grey colour.

It seems the drilling out of the old dental filling must have caused some debris spray and as she had her hands clenched across her chest, this spray got onto the links.

We now know that dental fillings include mercury, so don’t wear any gold during such procedures!

I have managed to use a metal polish wadding to get the gold colour back and I assume it was not too hard due to the minimal amount of mercury that is used in dental fillings.

We will let the dentist know so that he can advise patients to remove any gold under such procedures.

John Haas
– Brentwood, Essex, UK
^


August 15, 2017

A. And 15 years later:

Coconut oil will only give off some color so it looks like gold. The only way to get rid of the mercury is to boil it off. Mercury boils at 356 °C. Gold melts at 1060 °C, so do not heat it up that much. Remove any stones, etc. Use a propane torch, and be a little careful to not melt the gold. Keep it well ventilated, and do not breathe in the fumes.

Any high school chemistry lab would have everything you need.

This is by the way, the way the old goldminers did it.

Epi Log (fictitious)
– goldendale, California, usa
^


thumbs up sign Hi, thanks for the input. I doubt that you’ve used your real name as requested though, and your IP address is from outside the USA and apparently spoofed; so, although your advice might be good, we have to urge people to think very carefully about whether to follow it.
As you say, though, it’s “15 years later” and we’ve had not a single report from anyone that the coconut oil turned out to be only a temporary cure. Thanks again.

Regards,

ted_yosem
Ted Mooney, P.E. RET
Striving to live Aloha

finishing.com – Pine Beach, New Jersey



Need quick confidential answers? $25
Need project assistance? $100/hr.

August 2017
^

thumbs up sign I must be the luckiest person in the USA! When I watched, horrified, as the mercury from a broken thermometer spread over my 24 carat gold heirloom bracelet, I had no idea what I would do! I called a jeweler; he told me to bring it to him right away. Two days later I picked up the bracelet, restored! The jeweler is retired now, but I am forever thankful! I am submitting this note to let you know there are some jewelers who might help. Call the older ones in your community.

Susie Partin
– Louisville, Kentucky USA
August 17, 2017
^


Q. Can we boil the damaged gold ring in coconut oil by closing the pot’s top with a lid?

Aysha Fateena
– kilakarai, tamil nadu, india
February 10, 2018
^


February 2018

A. Hi Aysha. I don’t think it would hurt much to put a lid on the pot, but don’t do it inside, period.

Regards,

ted_yosem
Ted Mooney, P.E. RET
Striving to live Aloha

finishing.com – Pine Beach, New Jersey



Need quick confidential answers? $25
Need project assistance? $100/hr.

^


Before & after use of coconut oil, photos courtesy of Yesha Duggad:

13044-1b4

13044-1af

A. I broke a thermometer in the early 1980s and got mercury over my wedding ring. Our family jewelers cleaned it no trouble and at no cost. It was no big deal to them; this was in Mudgee NSW Australia at Byrnes Jewelers. I was very happy.

Maggie Consadine
– NSW Australia
May 16, 2019
^


thumbs up sign The coconut oil hack really works. I was repairing a BP instrument (Mercury) and a tiny bit of mercury touched my gold ring. I didn’t notice until I was washing my hands and panicked.
Searched on Google and came to this site. The coconut oil hack seemed the best one to try. Tried it and the ring was gold again. The polish was a little bit less yellow than previously.

Arun Agarwal
– Tura, Meghalaya, India
February 20, 2021

thumbs up sign Your method worked 100%. Good luck, Namaste.

Sampath Kumar Medavarapu
Astrologer – Kakinada
June 21, 2021

A. I accidentally exposed my gold ring to mercury and my ring turned while, I put my ring in a warm coconut oil (parachute oil easily available in India) and it worked well for me.
You have to take extreme caution not to inhale the fumes at any cost.

Aks singh
– Jodhpur India
December 31, 2021


sidebar

Q. Hi Ted, I wrote to you earlier before I saw that you had placed many replies on this website regarding the issue of Mercury on gold. I put my 22k ring in Tarn-x (said on the bottle good for gold!?) and it turned silvery white! Since it has diamonds in it I’m afraid to boil it in coconut oil so I’ve put it in very hot coconut oil but nothing’s happening so far. I’m not sure what chemical caused the reaction but Tarn-x contains THIOUREA, sulphamic acid, and detergent. Are any of these similar to Mercury in terms of causing such a reaction do you know?

Grace casale
Writer – Groton Connecticut
February 18, 2022
^

A. Hi Grace. You can get liver of sulfur from Amazon or eBay

⇦ on

eBay or

Amazon [affil link]

and probably from craft stores. But Tarn-X is very different from mercury, and liver of sulfur is very different from coconut oil as well, so I’m a bit confused :-)

Luck & Regards,

ted_yosem
Ted Mooney, P.E. RET
Striving to live Aloha

finishing.com – Pine Beach, New Jersey



Need quick confidential answers? $25
Need project assistance? $100/hr.