(1998)

I'm looking for a process to anodize titanium.

Does anyone know a vendor who supplies the chemistry

thanks, Ken

KEN CLAY

(1998)

Ken,

For the anodizing of titanium we use the following bath.

80 vol% phosphoric acid
10 vol% sulphuric acid
10 vol% water at room temperature.

The color of the anodic layer depends on the anodizing voltage.

Anodizing of titanium can also be done in 3 - 5 w% trisodium phosphate [linked by editor to product info at Amazon].

J.H. Pennings
TNO INSTITUTE OF INDUSTRIAL TECHNOLOGY


(1998)

Ken

I have had good luck using the trisodium phosphate [linked by editor to product info at Amazon] solution mentioned in another response, (3% to 5% by weight). My experience is in small parts of titanium and niobium and I get a large range of very vivid colors with this bath. One thing to remember is that the bath temperature should be kept below 80 degrees Fahrenheit otherwise the process breaks down and etches the workpiece. The resulting greyish surface is difficult to remove, and removal may cause an otherwise accurate part to become out of tolerance.

Howard Bailey

(2000)

I¥m looking for some people that have experience (Books, Publications,....) with : Anodizing Titanium Thanks

Taghezout
TU - Graz - Graz, Austria



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.