Anodizing Zinc Alloy Castings


(1998)

I have a ZA-12 sand casting that I need to be black in color as in anodized. I need to know the best process to do this and I need a vender that can perform this service. The casting weight is approx. 2 pounds and it is about 8" long.

Don Sherman
Marsh Co.


(1997)

How about zinc plate and black chromate?

pooky
tom pullizi signature
Tom Pullizzi
Falls Township, Pennsylvania



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.