topic 11876

White bronze plating

 

White bronze plating is used to replace Ni for the jewelry industry, what is the plating thickness?

WY Wong
- HK


 

Put 0.001 inches on it, and the jewelry will show up in antique shows 50 years from now. Put 0.00001 inches on, and like Broadway Gold, it will be the first thing to turn green in the spring.

pooky tom pullizi signature
Tom Pullizzi
Falls Township, Pennsylvania



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Comment to THIS thread START a NEW threadView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.