topic 11769

POR-15


 

Has anyone ever heard or used a product called POR-15, and does it work?

Bronte Devereaux
- Birmingham, Alabama


  POR-15 [linked by editor to product info at Amazon] is a great way to fix something rusty. It is easy to use and permanent. You did not say what you wanted to do with it.

Jeff Cleere
- Hattiesburg, Mississippi



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Comment to THIS thread START a NEW threadView CURRENT TOPICS



Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.