What does 333 on a gold chain mean? Is it 18k or 9k?

Kevin Ramcharran
- Jhb, South Africa


 

Karat stamps are parts of 24, so 18K is 18/24 and is equal to .75. The number 333 is the decimal equivalent to 8K.

Neil Bell
Red Sky Plating

supporting advertiser
Albuquerque, New Mexico
red sky banner ad



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Comment to THIS thread START a NEW threadView CURRENT TOPICS



Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.