Processing Aluminium in the Tricationic Zinc phosphate bath

 

While processing the load in a tricationic phosphate bath if the load contains a higher % of the aluminium, that dissolved aluminium will create any kind of the problem to the chemistry of the phosphate bath. Please explain the exact chemical reaction going on when any aluminium article is treated in the zinc phosphate bath.

Mr. Vaibhav Janardan Kulkarni
MARPOL CHEMICALS PVT. LTD. - Navi Mumbai, Maharashtra, INDIA



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Comment to THIS thread START a NEW threadView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.