Electroforming Process Set Up




 

Dear Sir,

I'm working on process "Electroforming", I wish to know about its applications & min. requirements to put a set up for manufacturing. I'm eagerly waiting for your valued reply.

Regards,

Paresh Deshpande
- Kolhapur, Maharashtra, INDIA



Electroforming is the same process as electroplating except that the substrate which has been plated is removed, and the plating layer itself becomes the functional part.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
 


Hi Paresh:

For detailed information on applications and requirements you might contact the Nickel Development Institute in Toronto, Canada. They will flood you with valuable information.

Good luck!

Guillermo Marrufo
Monterrey, NL, Mexico



Some of the items being made in India are Ice-cream factory moulds, Sugar Mill Meshes, imitation jewellery dies and moulds, etc. The cost for a plant should be within Rs 2.00 laks for a single tank prodn.line.

Khozem Vahaanwala
Khozem Vahaanwala
Saify Ind
supporting advertiser
Bengaluru, Karnataka, India
saify logo
 


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"