Electropolishing Tungsten



 

I am interested in finding a process that would be suitable for electropolishing Tungsten, including any pretreatment processes that may be required.

David Binks
- Bordon, Hampshire, UK



There are different methods of electropolishing Tungsten, the low-voltage method is pretty environmentally clean. It depends on the type of alloy you want to polish.

anna_berkovich
Anna Berkovich
Russamer Lab - Pittsburgh, Pennsylvania
(ed. update July, 2025: sorry, Anna has retired)



I'm also looking to electropolish tungsten, specifically tungsten-rhenium.
Information on the electrolyte and its concentration, current density etc would be very helpful

Maryanne Muriuki
- Somerville, New Jersey
May 12, 2008


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"