topic 11011

Tarnishing Copper


 

Hello,

I am in the process of building some tables with copper tops. However, I do not like the "shiny" finish. I am not trying to achieve a verdi gris finish, just a more tarnished appearance. Is there any way I can speed up the process?

Elizabeth Jackson
- Marlboro, Massachusetts

Ed. note: Please see our FAQs on this topic.



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Comment to THIS thread START a NEW threadView CURRENT TOPICS



Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.