Alodine/Iridite Touch-up Process

 

I would like to touch up a part that has been Alodine/iridite coated. What product should I use to maintain a Mil-C-5541 [link by ed. to spec at TechStreet] standard? What is the MIL-STD for touching-up of aluminum? Thank you for your quick reply.

Craig Meyers
- E. Aurora, New York


 

Products approved for MIL-C-5541 are listed on QPL-81706 [link by ed. to spec at TechStreet].

Chris Jurey, Past-President IHAA
Luke Engineering & Mfg. Co. Inc.
supporting advertiser
Wadsworth, Ohio

luke engineering banner



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Comment to THIS thread START a NEW threadView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.