Electropolish 420 ss


 

Can anybody help me on the best solution for electropolish aisi 420 ss?

Flavio Stramare Ribeiro
- Curitiba, Brazil


 

Stainless 420 can be electropolished in non-aggressive solution, but higher power is required.

anna_berkovich
Anna Berkovich
Russamer Labs
supporting advertiser 
Pittsburgh, Pennsylvania
russamer labs banner


 

Try a search of this site under that subject. That would be a good start for anyone.

Best Wishes,

tom pullizzi portrait
Tom Pullizzi
Falls Township, Pennsylvania



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Comment to THIS thread START a NEW threadView CURRENT TOPICS



Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.