An ongoing discussion starting in 1997 . . .


Q. Hello,

I need to know some place to learn hard chrome plating (training), I would like a school more practical and less theoretical, I have some books and the equipment necessary.

Please send me the phone, address, and the contact.

Remberto Brito
- Columbia


A. I only know Kushner Electroplating School, Sunnyvale, California.


Tony Rodriguez
chrome plating - Columbia


A. AESF ( periodically offers a class on chrome plating. SME used to have a class. Both of these are mostly theoretical with some practical, but no hands on. You are from the same country. Could you possibly give Remberto some hands-on help at your facility. He is a beginner in chrome and would appreciate any help that you might be able to provide. Jim

James Watts
- Navarre, Florida

Hard Chromium Plating
by Guffie
from Abe Books


A. Hi Remberto. If you can get to the U.S.A., Hard Chrome Plating Consultants, Inc. in Cleveland offers (or offered) specialized hands-on training classes in hard chrome plating. It included a 362-page looseleaf book "Chrome Plating Simplified - Reversible Rack 2 Bus Bar System" which is extremely detailed and might be available by mail. They also offer (or offered) the course on VHS tape. Good luck.


Ted Mooney,
Teds signature
Ted Mooney, P.E.
Pine Beach, New Jersey

To minimize searching and offer multiple viewpoints, we've combined multiple threads into the dialog you're viewing. Please forgive any resultant repetition or failures of chronological order.


Q. I am looking for books or video training that explain chromium plating in a practical and easy to understand format especially in Anode design, Jigging, troubleshooting in plating bath. Any information is greatly appreciate, thanks.

David Ackley
- Peoria, Arizona, USA


A. Talk to the folks at Hard Chrome Plating Consultants in Cleveland, OH.

The author, Clarence Peggar, died a few years back, but junior is running the business the last I heard.

The book is full of bad mouthing regular chrome plating, but if you can ignore the BS, it is a wonderfully practical book.

I am a fan of conforming anodes and they will work in a regular tank also. I happen to think that the two bus bar method is superior to normal plating methods, but that is my opinion.

They sell a video set also. This is basically his school put on tape. I have never seen it, so can not comment on it. Did go to the school many years ago.

James Watts
- Navarre, Florida


A. I also have Clarence Peger's book, and I highly recommend it as a reference resource. The book is titled "Chrome Plating Simplified - Reversible Rack 2 Bus Bar System" and is published by Hard Chrome Consultants LTD, Cleveland, Ohio.

Ralph Peltier
- Providence, Rhode Island


A. Hi ,

The AESF & Atotech both sell a CD dealing with this subject. The AESF also runs a training course on Functional (read Hard) Chromium Plating, check out their web site for details of where & when the course is to be held. Also there are some terrific articles written by Dr. Ned Mandich published (within the last 18 month or so) in Metal Finishing magazine which give some really practical answers to running & troubleshooting Chromium plating solutions.


John Tenison-Woods
John Tenison - Woods
- Victoria Australia

This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site


Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices

©1995-2018, Inc., Pine Beach, NJ   -   About   -  Privacy Policy
How Google uses data when you visit this site.