Immersion Plating Tin onto Steel




Q. Is it possible to get an immersion coating of tin on to steel from an alkaline stannate solution, containing cyanide?

Uwe Berger
1998


A. Durney's Electroplating Engineering Handbook this on eBay, AbeBooks, or Amazon [affil link] gives such a formula on p. 422.

tom pullizzi monitor   tom pullizi signature
Tom Pullizzi
Falls Township, Pennsylvania
1997


A. Hi. The tin is added in stannous form (SnCl2):

alkaline stannate immersion bath

-- but not being a chemist I think I'll agree with Tom that it's an alkaline stannate bath nonetheless.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
July 2013


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"