Clearcoat for gold plated products?


(1998)

I am looking for a hard clear coat for gold plated products. I was told there was a product called Clear Chrome but I am unable to find a supplier. If you know where I can get this product...

Christopher J. Harvey
- plating shop


(1997)

We use "Clearlyte" electrophoretic lacquer supplied by Enthone-OMI/Sel-rex for clear coatings on gold and silver plated items suggest you contact your local agent

Regards

bob lynch
Bob Lynch
     plating company
Sydney, Australia



(2000)

hi, We are having trouble sourcing "ERCALENE" LACQUER PRODUCED IN UK (I THINK) OUR PERTH, WESTERN AUSTRALIA, SUPPLIER IS HAVING TROUBLE ALSO - CAN ANYONE SUGGEST WHERE I CAN PURCHASE. WE USE IT TO COAT POLISHED BRASS. THANK YOU. TOM

THOMAS MILLAR
- PERTH, WESTERN AUSTRALIA



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.