Patina finish on brass


(1998)

Looking for a metal finisher to provide a patina finish on brass bands approximately 3" high and 18" in diameter. Prefer supplier that is close to the state of Ohio...

Gary T [last name deleted for privacy by Editor]
lighting corp - Ohio
outdated


(1997)

Dear Gary,

To find a supplier, contact a local plating supply company or the Ohio Metal Finishing Association, or the American Electroplating Society. They should be able to help you.

Gary Patigler
electroformer - Richmond, California


(1997)

Geez. What are WE, chopped liver or something? smiley

An easy first step is to consult the list of plating shops here at www.finishing.com/shops/

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.