Measure reflectivity of mirror polished stainless surface


(1996)

What is the best way to measure reflectivity of a mirror polished stainless surface?

Does anybody know what is the reflectivity numbers for a regular glass mirror?

Mike

Michael Liu Taylor
Michael Liu Taylor
   specialty stainless steel distributor
Dallas, Texas



(1996)

We use a Solar spectrum reflectometer,Manufactured by Devices and Services Co. Dallas, Texas.

Reflectivity of a regular glass mirror is R am2 = .882

Hope this helps,

Max T. Faeth
- Los Angeles, California, USA


(1998)

Thanks Max.

Our interested customer performed their tests using:

Helium Neon Laser at 633 nanometer wavelength

Results: 63-64% reflectivity on Super #8 mirror polished stainless
and 56-57% reflectivity on Super #8 mirror polished stainless
with titanium nitride (gold color finishes).

I'm told these number is below regular glass mirrors...but very good for mirror polished stainless surface.

Michael Liu Taylor
Michael Liu Taylor
   specialty stainless steel distributor
Dallas, Texas


(1998)

R&D division of Kombassan Holding is working on the development of a solar energy system.

We plan to commercialize the system within the next couple of years.

I want to measure mirror surface's reflection efficiency. I learned that reflectometers used on this subject, we want to buy one. We need a portable reflectometer. I want to get detailed technical information.

Is there a distributorship in Turkey? Could you send me catalogues, price list and brochures.

Thank you very much in advance for your help.

Sincerely

Fiener Keskin, Optic Group Leader
- ANTALYA, TURKEY


July 13, 2010

To: Max T. Faeth

Hello! I have a question about the equation R am2 = .882. What do the variables represent (R, a, m). Also is that m^2? Thanks!

Dan Guardia
- New York City, New York, USA



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.