topic 516

Rochelle copper plating properties / bath contents


(1996)

May I kindly request of Rochelle copper plating's property / bath contents and data, otherwise advise reference book? I am very happy to join in line if you need my help but I should learn more before , thus, first your help is needed. By sae

(Miss) Sae.y.oh
- Korea Industrial Technology Research Institute


(1996)

Formulation for Rochelle Copper plating :
copper cyanide 6 oz/gal
sodium cyanide 7.5 oz/gal
sodium carbonate 4 oz/gal
sodium hydroxide 1 oz/gal
sodium potassium tartrate (rochelle) 6 oz/gal
Pratt & Whitney spec. PS309.

Dave Brackenridge
aerospace plating - Germiston, South Africa



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.