netneut
finishing.com -- The Home Page of the Finishing Industry
A website for Serious Education, promoting Aloha,
& the most FUN smiley you can have in metal finishing


Finishing.com has been free for 22 years,
but without net neutrality we could soon
cease to exist. Do us a solid, click on
the banner, and contact congress today!
HomeFAQsBooksHelpWantedAdvertiseForum
topic 463

Need smoother nickel-iron plating


(1996)

I AM LOOKING FOR A SOLUTION TO REDUCE THE SURFACE ROUGHNESS OF NiFe PLATING.

THE ROUGHNESS I HAVE NOW IS ABOUT 50A BUT I'D LIKE TO REDUCE TO 5A. DOES ANYBODY HAVE ANY QUICK SOLUTION TO THIS? I WOULD APPRECIATE IT VERY MUCH.

STEVE CHIEN



Atotech sells Nickel-Iron Plating additives which give smooth bright deposits over a wide current density range. I don't know if your application allows the use of organic brighteners, or even if brighteners will help your surface roughness readings.

pooky
tom pullizi signature
Tom Pullizzi
Falls Township, Pennsylvania



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.