Remove scratches, re-polish Porsche 914 wheels aluminum wheels


(1996)

I recently bought aluminum forged rims for a Porsche 914. there are some slight scratch marks on the polished aluminum. I would like to remove the scratches and then repolish the aluminum accents on the wheels. any suggestions on how I might go about this would be appreciated.

Chandler [last name deleted for privacy by Editor]


(1996)

Hi, Chandler. I don't know the specs for these wheels--whether they are anodized, or coated with an organic. But in any case they are not going to be just a plain bare aluminum, so you have to deal with the coating first. You will see threads here about removing anodizing as well as clear coating. We have many threads on line here about polishing aluminum; probably letter 800 is a good place to start for instructions. Good luck!

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.