Formulating an EN (Electroless Nickel Plating) Solution


(1996)

I am trying to make Electroless Nickel Solution for my own use. However, My home-brew solution can only last for 3 turnovers. I am using Malic Acid and Amino Acetic Acid as the complex.

I would like to get in touch with anybody who has experience in this field and your help is very much appreciated.

Thank you.

Peter L [last name deleted for privacy by Editor]
- Singapore

Chemical (Electroless) Nickel Plating
G. G. Gawrilov

Electroless Plating
Mallory & Hajdu

November 24, 2008

Hi, Peter. I am pretty sure that you can get the information you need from Gawrilov's "Chemical (Electroless) Nickel Plating".

If anyone wishes to refer you to other literature which they think will help, we'll be happy to list those references. But considering the anonymity of the internet, we can't actually print formulation information here because we have no way of determining what is legitimately owned versus what may be trade secrets. So peer-reviewed published literature may be the way to go. Good luck.

Regards,

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.