What does porosity in chrome plating look like?


(1996)

I am looking for a source of a picture demonstrating,though magnification, the porosity of a chrome plated surface. Thank you.

Richard Staehle



Hard Chromium Plating

(1996)

Can we assume you are referring to hard chrome plating as opposed to decorative nickel-chrome plating, Richard? I'd say it resembles a dried mud flat. There are a number of texts on chrome plating which show what it looks like, and the 'Handbook of Hard Chromium Plating' by Robert Guffie would be a place to start. Good luck.

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.