Determining sulfate in aluminum anodize


I am trying to determine the amount of sulfate contained in the anodic coating when anodizing aluminum in 12% sulfuric acid. Is sulfuric acid consumed in any other way in the anodizing solution?

I can not find any literature that will address this issue.

Thank you

Art Sanders


Surface Treatment & Finishing of Aluminium and Its Alloys
Wernick, Pinner & Sheasby

See our book section for some basic references on anodizing and/or zip over to Anodizer's Plaza, a web site in Japan, written in English, and available under our WWW links. See my response to your letter #287 for two references.

The Canning Handbook is another, the Garden State Electroplating Manual is another.

tom pullizzi monitor
Tom Pullizzi
Falls Township,
   Pennsylvania 

----
Ed. note: Regrettably we are no longer able to find the Anodizer's Plaza website.



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.