EN to polymer Bonding



A discussion started in 1996.
Add your Q. or A. to restore it to the "Current Topics" discussions.

(1996)

I am researching into the bonding of electroless nickel plate to polymer coatings, and have failed to find any references - even to polymer - metal(any!) bonding. If any one out there has any suggestions of literature/web pages, etc. it would be a great help.

Thanks

Monica Tomlinson
The University of Edinburgh


G.G. Gawrilov's little book, Chemical (Electroless) Nickel-Plating, Portcullis Press, Redhill, 1979, Queensway House, 2 Queensway, Redhill, Surrey, RH1 1QS. In English, ISBN 0 86108023 8 is big on content, with references from around the world. See chapter 13, Chemical Nickel-Plating in Relation to the Carrier Material.

pooky tom pullizi signature
Tom Pullizzi
Falls Township, Pennsylvania



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Comment to THIS thread START a NEW threadView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.