Tearing of Aluminum Extrusions During Buffing Operation


(1996)

We are having a problem in our finishing Dept. of our Aluminum extrusions tearing open during our buffing operation. We have had problems with die pick up as well as die tear up but have gotten a handle on these problems. We feel that material is being tore open during our buffing operation. We have made some progress by correcting some minor problems, and reduced the tearing of our extrusions. I have contacted our suppliers but have had no success in solving our problems. If you could identify or direct me to a source, it would be much appreciated. Thank You.

lglove [last name deleted for privacy by Editor]

(1999)

get as much grease on it before buffing then use a bias buff with a color compound; work it, but not to hard . I run into a lot of crazy stuff. there is a way to fix your trouble . hard to say on here.

terry sheckles
racine Wisconsin


(2001)

Give a dip in nitric acid after anodizing i.e., after sealing and then grease it well before buffing

Khalid M Bhatti
- Pakistan



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.