Letter 9080

NEED HELP ON MIL-SPECS TO 93/7 SOLDER BATH? 

+

I HAVE A QUESTION FOR ANY ELECTROPLATING ENGINEER. WE DO 60/40 SOLDER PLATING AND TO MIL-P-81728, ONE OF MY CLIENTS REQUESTED THAT I LOOK INTO 93/7 TIN-LEAD BATH. MY QUESTION IS UNDER WHAT MIL-SPEC DOES THIS 93/7 BATH FALL UNDER? I HAVE LOOKED INTO MIL-T-10727 AND MIL-P-81728 ALSO ASTM-P-81728, MIL-F-14072 AND NONE OF THIS WILL FALL INTO THE 93/7 BATH.

ANY FEEDBACK WOULD BE HELPFUL,

THANKS,

JOE LUPERCIO
- LOS ANGELES, CA.