How do Acids Clean Pennies?


I'm a sixth grader, and I'm doing a lab about cleaning pennies right now. I used stuff like vinegar ⇦ in bulk on eBay or Amazon [affil link] , lemon juice, and lime soda because I heard that acids clean pennies better. How do the acids clean the pennies?

Stephi
- Palo Alto, California, USA
2001


Yes my 4th grader has a project on solutions that cleans pennies - I need to know what type of solutions does this - and any idea on how we can present this project.

Bobbie Hereford
- Atlanta, Georgia
2003


A lemon with some salt will clean a penny.

Vexx E.
- New York City, New York, America
2003


A lemon will work but personally vinegar works better cause I am doing a penny experiment in the 8th grade and that is what we used we soaked pennies in vinegar for about 5 minutes we took the pennies out and they were clean. You know what? Ketchup works also.

Kaoru-Dono
- Cold Spring, Kentucky, USA
2003


I am also doing a science fair project about which liquids clean pennies the best. I tried to clean pennies with vinegar and it worked pretty well. I tried to clean a dollar coin and some silver coins with vinegar and it made a darkish brown stain. I guess vinegar is too strong of an acid to clean other coins with.

Minh P.
- Savannah, GA, USA
2003



Ed. note: Please see our F.A.Q. on the subject.

Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"