Letter 8072
Seeking technology for silver plating
aluminum
+
I need technology for silver coating Aluminum.
Goran
Lavica Komerc - Belgrade, Yugoslavia
+
I DIDN'T KNOW CLEARLY WHAT YOU MEAN BY COATING BUT IF YOU MEAN
ELECTROPLATING THEN I THINK THIS PROCEDURE WILL HELP
1-CLEAN THE SURFACE OF ALUMINIUM
2-ETCHED IT WITH [SODIUM HYDROXID]
3-IMMERSE IT IN ZINCATING SOLUTION
4-REMOVE ZINCATING BY NITREC ACID
5-ZINCATING AGAIN
6-ELECTROLESS NICKEL
7-ACIDIC COPPER
8-NICKEL
9-SILVER PLATING
RAFAAT ALBENDARY
NATIONAL PLASTIC ELECTROPLATING - CAIRO, EGYPT