Letter 8039
Acid copper with higher
thickness
+
My acid copper plating plant can't do 200 to 250 microns plating.
It takes too much time to do high thickness plating. Plating also
pilling after getting thickness. Have you any process to get
thickness speedily without pilling?
Vinay Talsania
Deoki manufacturers - India
Dear Reader, please --
- Post a
question on a different subject.
-
- Answer this question (in non-commercial
fashion).
-
 |