Letter 8034
White Rust
+
I have a Lester Building and I have white rust along the bottom of
my building. Butler Buildings sent out someone from Valspar Corp. who
did the paint on the building. He said that I have white rust. He
said that it was caused by using weed killer along the building. He
said that the sun and the weed killer not being washed off the
building was the cause of the white rust. He said that they might
repaint the building for me. So I went to the internet and checked
out white rust so this is why the email.
My question is why did the weed killer cause the white rust? What
do they have to do so that the white rust does not come back?
Thanks
Ed Mayhew
- Colona, IL
Dear Reader, please --
- Post a
question on a different subject.
-
- Answer this question (in non-commercial
fashion).
-
 |