Recycling spent die strip
caustic
+
I have been working with Brian Tomkins on the use of 308A die
strip additive to speed up the stripping of dies and the trials were
successful. Brian further proposed the use of the spent die strip
caustic in anodising etch operation, something we are currently
pursuing. I would like to know the further additives that we need to
use to prevent the adverse effect of the dissolved aluminium carried
over from die strip. Currently we are using almeco plus 2 to hold
aluminium ions in solution in our anodising etch but we are having
problems on the accumulation of sludge in the etch tank which is
affecting the heating up of the tank.
Please can you suggest an alternative.