No passwords, no registration, no paywalls, no popups, no AI

As an Amazon Associate & eBay Partner we earn from affil links

Home /
T.O.C.
Fun
FAQs
Good
Books
Ref.
Libr.
SITE
NEWS
Help
Wanted
Current
Q&A's
Site 🔍
Search
finishing.com -- The Home Page of the Finishing Industry Search our quarter-million Q&As

Home of the finishing HOTLINE since 1989

-----

Greenish Color on Anodized Parts





I have to go out for quotes for anodizing our aluminum housings per Mil Spec: MIL-A-8625 / MIL-PRF-8625 [⇦ this spec on DLA] TYPE II CLASS I. When I look at our parts that have had this process they appear to be a greenish color. However, when I read the Mil Spec it mentions the fact that it is a non-dye process. Does the sodium dichromate dip/process produce the greenish color?

RICK FABRIZI
- Lanesboro, Pennsylvania - U.S.A.
2001



Yes. It's not a dye, but it is greenish.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
2001


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"