-----Aluminum in Zincate bath
Does anyone know if there is a way to remove the aluminum from a zincate solution?
Abgie Molnar- Fort Saskatchewan
2001
Abgie,
I would try with electrolysis, because exchange resins keep both Aluminium and Zinc. I found this site: www.tinaja.com/glib/muse114.pdf
Good luck and let me know

Francesco Cicchetti
- Sulmona, Italy
2001