I am looking for process to put copper bottom on stainless steel utensils. I am looking for simple process. Any help will be appreciated
Kishor ValiaK. Valia & Coy. - Mumbai, India
2000
I know this can and has been done by copper electroplating to controlled depth. I don't know if there is any other available process such as laminating.

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
2000
It maybe possible to weld the copper on during production. If the utensils (pots?) are drawn out from a stainless steel stamps then if a smaller copper stamp were aligned below the steel one it could bond to the steel during drawing. I'm no expert on this, but this could be an avenue worth looking into.
Ian
university - Glasgow, Scotland
2001
Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!