-----Does Iridite fluid contain TCE?
Could waste Iridite fluid used in the metal fabrication business contain any chlorinated solvents such as TCE?
Brian Diepeveen- Mount Olive, New Jersey
2000
2000
You should get an MSDS and tech data sheet from the manufacturer to settle the question, but I should certainly think not.
Does the work go through a vapor degreaser before conversion coating?

Ted Mooney, P.E.
Striving to live Aloha