Letter 6087

Copper roof aging unevenly 

.

We have a copper roof over our bay window. It is about 15 years old. The front half of the roof is green, while the rear half is brown/red tones. Over the years, when water has spilled out from the second story gutter above, it has caused the roof to discolor and age unevenly.

Is there any way to even out the color to be either green or brown/red?

Is it possible to "seal" the copper roof so this doesn't happen again over time?

Tracy S name was deleted
- Kernersville, North Carolina


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
Post a new question or inquiry on a different subject.


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com