Hot dip aluminizing books &articles 

.

I am a student who is working on the effects of flux in hot dip aluminizing. I need the names of some books or articles about it.

ma sha
- India delhy


++++++

Type II hot dip aluminized steel: performance in storm drains or pipes?

Peter Elliott
Consultant - Colts Neck, New Jersey, USA


++++++

There is a fourteen-page chapter on "Aluminum Coating of Steel" in ASM Metals Handbook, Ninth edition, Vol. 5, "Surface Cleaning, Finishing and Coating". The newer edition "Surface Engineering" may have some of the same information scattered through it, but it is not accessible as a chapter.


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


Dear Reader, please --

Post a question on a different subject.
 
Answer or follow-up on this subject (in non-commercial fashion).
 

 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com