430 series stainless steel electropolishing  

Electropolishing  
services pointer 

       
February 5, 2010

My name is Geeno from Bangkok,

Pls, help me how to electropolish 430 series. I try to electropolish but it not look good like 304 series . I use Phosphoric and Sulfuric for 430 series but, it not work at all. It work with 304 series. Pls, help me what chemical I should use to electropolish 430 series

Thank you

Geeno Wong
student - Bangkok, Thailand
  ^- Privately contact this inquirer -^
February 16, 2010

I have electropolished stainless steels, mainly 304 & 316. I have tried electropolishing 400 series stainless steels, but they do not develop the highly bright finish that 304 & 316 achieve when electropolished using solutions containing phosphoric and sulfuric acid. I believe the Electropolishing Engineering Handbook lists some formulas for 400 stainless steel elcectropolishing. Also some of the suppliers in this forum I believe market 400 series stainless steel electropolishing processes.

Thomas Kemp
- Cleveland, Ohio, USA


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search