53371
Seeking Brass Dip [Texas]
October 15, 2009
I am looking for a product such as Brass Dip that was supplied by
Paxton Production Supply. They no longer exist and I am now looking
for an alternative to what this brass dip did. It coated the brass
with a bright yellow pickeled finish that would not tarnish after
being dipped in the solution for only 10 to 15 seconds. It came in a
crystal form and was added to water to make up the solution. After
dipping in brass dip the casting was then dipped into Nitric acid for
only a couple of seconds to finish the polishing process.
Could anyone please direct me to this product or another that is
similar.
Dennis Mashburn
buyer - Abilene, TX, USA


-
 |