Need White RoHS compliant Paint for Zinc Cast Parts

August 17, 2009

I am looking for RoHS compliant White, mate finish paint that could be applied to a small square area of the zinc cast part. Mostly paint would be applied with brush/applicator.

Since our products are sold to industrial application. Usually reliablity of the paint- 50,000 hrs with temp. -20 deg. C to 70 deg. C thermal resistance- must. Paint should not peel of over period of time.

Any suggestion on supplier of the paint? Grade/Type etc. Would be appreciated.

Sam

Sam Sam
Engineering and purchasing - Fremont, California, USA
  ^- Privately contact this inquirer -^



----
Readers: This site is made available for camaraderie & technical info exchange by our supporting advertisers, and they will contact the inquirer privately regarding their commercial needs. Please offer comments on any technical issues, but not sourcing suggestions or testimonials. Thanks!


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search