Need Source for Aluminum Coating per MIL-C-83488  

June 22, 2009

We are looking for a source to Aluminum Coat per MIL-C-83488, Class 3, followed by a Solid Film Lubricant per MIL-L-46010, Type I. The parts are 6AL-4V Titanium, 5/16 diameter x 1" long (clevis pins). The quantity is 2500 pcs..