52352

Pickling paste without hydrofluoric acid  

June 10, 2009

Is there a pickling paste available for post weld finishing of stainless steel available with no hydoflouric acid.Im aware of <0.5% pastes but not Zero hydrofloric.

We produce a mobile electropolisher so are interested in developments in pickling paste

Richard Ray
manufacturer of post weld finishing machine - Ballina, NSW, Australia
contact button


June 30, 2009

This is a very difficult task. He have successfully developed green" pickling pastes without nitric acid for stainless steel, carbon steel, titanium. We are currently working on eliminating hydrofluoric acid also. However work is not completed yet.

Anna Berkovich
Russamer Lab

Pittsburgh, Pennsylvania


Dear Reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com