52154
Verification Tests for Cobalt Chrome
Passivation
May 12, 2009
Hi All,
I work for a manufacturer of We currently passivate a range of
stainless steels in Citric or Nitric solution (depending on customer
requirements) and use Copper Sulphate and Boil tests as verification
methods.
We are now looking to passivate some cobalt chrome implants in Nitric
Acid. Can anyone suggest any verification methods for testing the
effect of the passivation on cobalt?
Thanks
James Dodds
Quality Engineer - Sheffield, United Kingdom

June 2, 2009
James,
Passivation tests for stainless steel are checks for the presence of
free iron on the surface, and you would want a passivation test for
non-ferrous alloys such as your cobalt chrome to do the exact same
thing. Go ahead and use copper sulfate and/or the boil test.
-
-
 |
|