52118

Chemical polishing Invar before plating with silver  

April 9, 2009

Can anyone recommend a chemical cleaning process to turned invar components before they are plated with silver? I am concerned with etch pits, etc., to an existing process which was not developed for invor but for kovar material.

Raman Mistry
Product designer - Southampton, UK