Seeking reel to reel plating of selective
gold on 6 inch wide strip.
May 12, 2009
We seek a plater who can process .0321" thick C26000 H02 Temper
reeled product. The parts would receive nickel allover followed by
two gold zones. We could provide with a single external carrier or
two external carries for masking or similar selective plating
process. Alternately, we could provide a carrier in the center of the
parts to allow for controlled depth plating on each end of the strip.
We would need to qualify the plater quickly before sharing a print.
This would probably represent approximately $40K - 80K in stamping
business annually for this first part, plus gold.