Hard chrome at very low temperature working conditions

May 12, 2009

Dear friends,

would there be a problem to internaly (dia Ö112mm) hard chrome plate a stainless steel [SS-316 (AISI-B8M)] sleeve, that works at a temperature of -164 Celcium degrees?

Thanks in advance

Chris Sigalas
Met. Eng. - Athens, Greece
  ^- Privately contact this inquirer -^

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search