Tarnish of electroless nickel over brass or alum. when ultrasonic aqueous cleaning  

May 7, 2009

We have thousands of parts Electroless Nickel plated and often they look fine before cleaning in a multi-stage ultrasonic cleaner. However, after processing in the ultrasonic cleaner (two stages of ultrasonics, one rinse, one dry -cleaner is Blue Wave Detergent # 25-I, 4 parts purified (Seattle city water through filters) deionized water to 1 part liquid detergent)). Many of the parts come out with brownish to blackish spots of irregular shapes. They kind of look like the variation you would get with water spots. Strangely, if we don't turn on the ultrasonics, we don't have this staining issue (though we have to soak them longer to get fingerprints etc. off of them). We are trying to get them clean for oxygen service. The brownish/blackish spots can be buffed off but that is labor intense and thins the surface.

 

Ed Huncovsky
Customer - Kirkland, WA, USA
contact button


Dear Reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com