Etching of an enhanced Aluminum coating on a UV fused Silica substrate

April 29, 2009

I would like to know how to etch an enhanced aluminum coating on a UV fused silica substrates of square, circular, rectangular shapes which typically etch a minute portion to be etched like polka beam splitter.

Lakshmana Kumar
- Bangalore, Karnataka, INDIA
  ^- Privately contact this inquirer -^

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search