51092
Seeking 2.5 mil Cu plating of 30 pcs. of
316SS aprox. 10"X12"x3/16"
January 29, 2009
We need to plate 30 pcs. of 316 SS to a thickness of .0025 with
Copper. The copper then needs to have a flash coating of nickel. Each
piece to be plated is curved in two dimension. Total dimensions are
approx. 10"x24"x3/16", but only half the piece is to be plated. The
rest of it will need to be masked. We are located in NYC but are
willing to ship.
Nicholas Rivera
research lab - New York City, New York, USA


-
 |